Post Time:Jun 08,2016Classify:Company NewsView:747
Skewback on crown of chauffer 1#~5# on the south and north sides of the arch angle in the melting pool of the float glass furnace was seriously eroded; skewback bricks had been melted completely and the outside of the skewback had turned red; downward of the skewback steel was exposed to the flame, posing a serious threat to the overall safety of the crown. By using the company’s ceramic welding technology and induction ceramic welding gun technology, the damaged portion was repaired, so that the structure safety of the furnace was ensured and the service life of the furnace was prolonged for another two years!
Source: unknowAuthor: unknow